Archive Results for tensile testing : 6 Buying Leads (BEFORE January 1st, 2015).
- 11 Nov, 2014
- Dear Sir/Madam,
please send quotation of blow film grade recycle LDPE granules.
Item Test Method Value Unit
Density ASTM D-1505 0.920-0.922 g/cm3
Melt Flow Rate (MFR) ASTM D-1238 2.1-2.9 g/10min
Tensile Strength at break ASTMD638
Breaking elongation ASTMD638 500 %
Tear strength MD ASTMD638
Tear s
- This buyer would like to receive quotations from Premium Members only.
-
Categories : Rubber & Plastics, Recycled Plastic
India
- Contact Now
- 28 Mar, 2011
- Tensile testing facility up to 60 tons.
Stress - reliving
Patenting.
Bell type annealing.
BIS LICENCES HELD : IS:1856-COLLIERY HAULAGE WIRE ROPE
IS:2266-ENGINEERING WIRE ROPE.
IS:6003-PRESTRESSED CONCRETE WIRE,
BS 5896, NORMAL RELAXATION.
IS:6006-PRESTRESSED CONCRETE STRAND OR BS 5896/ ASTM A 910
-
Categories : Minerals & Metallurgy, Steel Wire
India
- Contact Now
- 20 Sep, 2010
- Specification
We require following material very urgently.
1) Steel Rod Dia 7mm (+ 0.5mm)
Material:
steel confirming to IS 4454, part-III(Grade IS)
OR
steel confirming to 8052-2006(Grade 50Cr+V2)
2)Properties:
1. Tensile Strength-Minimum 150Kg/mm2(Test shall be carried out in accordance with IS-15
-
Categories : Manufacturing & Processing Machinery, Other Metal Processing Machinery
India
- Contact Now
- 31 Mar, 2010
- IS 1079 for HRCSS
IS 513 for CRCSS
Test Specifications
2.2.1 IS 228 - Test method for chemical analysis of steel
2.2.2 IS 1608 - Test method for tensile strength of steel
3.7 Supplier Responsibility
3.7.1 Any steel sheets supplied to MPPL shall be tested according to our material
test procedure a
-
Categories : Minerals & Metallurgy, Steel Sheets
India
- Contact Now
- 26 Oct, 2005
- Tensile strength: 4 - 5 Newton / meter
8. Solid colour not liable to change
9. Bright colour and soft finish
10. The thread should be treated and has a degree of humidity and a material that should be added to prevent static during textile
11. The required colour: (Brown, Beige, Red, Blue, Pink, da
-
Categories : Textiles & Leather Products, Synthetic Fiber
India
- Contact Now
- 28 Jul, 2003
- Tensile Strength : 52-62 Kgf/mm2
3) Elongation : Greater than 22 %
D. Process used by us to manufacture the Cylinder: Hot spinning.
We request you to forward us your most competitive offer along with product catalogues and client list. Test certificate are to be supplied with every consignment. Our
-
Categories : Minerals & Metallurgy, Cast & Forged
India