<title><![CDATA[DIN 1.2379 Cold Work Mould Steel Bars with ANSI D2 Steel Grade]]></title><link><![CDATA[https://fushunharrislee.en.ec21.com/DIN_1.2379_Cold_Work_Mould--11359578_11359579.html]]></link><description><![CDATA[1.40-1.600.10-0.600.10-0.600.030 max0.030 max11.0-13.00.70-1.200.50-1.10
6 1.2379 HEAT TREATMENT:FORGING: 1.2379 Heating for forging must be done slowly and uniformly. Soak through at 1850°-1950°F ]]></description><pubDate><![CDATA[20210329]]></pubDate></item>
<item>
<title><![CDATA[S17400,SUS630,ASTM630,17-4PH Stainless Steel Round Bar]]></title><link><![CDATA[https://jyxctg.en.ec21.com/S17400_SUS630_ASTM630_17_4PH--7086713_7086714.html]]></link><description><![CDATA[1.40~1.60
&amp;le;0.60
&amp;le;0.60
11.00~13.00
0.70~1.20
&amp;le;1.10
&amp;le;0.030
&amp;le;0.030
&amp;le;1.00
The main properties: 
1. The hardness after D2 tool steel annealing Less than or equal 255 HBS.
2. D2 tool stee]]></description><pubDate><![CDATA[20131015]]></pubDate></item>
<item>
<title><![CDATA[STD11 Cold Work Alloy Tool Steel]]></title><link><![CDATA[https://otaisteel.en.ec21.com/STD11_Cold_Work_Alloy_Tool--9723517_9947724.html]]></link><description><![CDATA[1.40～1.60
Si(％)
&amp;le;0.40
Mn(％)
&amp;le;0.60
P(％)
&amp;le;0.030
S(％)
&amp;le;0.030
Cr(％)
11.0～13.0
Mo(％)
0.80～1.20
V(％)
0.20～0.50
Ni(％)
&lt;0.50
Equivalent of KS STD 11 cold work alloy tool s]]></description><pubDate><![CDATA[20160427]]></pubDate></item>