<title><![CDATA[material 4340 | Material 4340 Thermal Properties | China Material 4340 Steel Round Bars]]></title><link><![CDATA[https://4340steelplate.en.ec21.com/material_4340_Material_4340_Thermal--11570260_11592434.html]]></link><description><![CDATA[4340 Steel Round Bar Sheet Plate Heat Treatment and Process
Stress RelievingFor pre-hardened steel stress relieving is achieved by heating steel 4340 to between 500 to 550°C. Heat to 600 °C – 650]]></description><pubDate><![CDATA[20220624]]></pubDate></item>
<item>
<title><![CDATA[1.3243 High Speed Steel | AISI M35 DIN 1.3243 High Speed Steel Storehouse]]></title><link><![CDATA[https://songshunsteel.en.ec21.com/1.3243_High_Speed_Steel_AISI--11800483_11800914.html]]></link><description><![CDATA[is lower than 500℃. Then heat to 840-860℃, keep the temperature for four to five hours. Furnace cooling to 500℃ below than out of it. Cooling slowly in the annealing furnace. After the annealin]]></description><pubDate><![CDATA[20230602]]></pubDate></item>
<item>
<title><![CDATA[AISI H13 DIN 1.2344 SKD61 Hot Work Mould Steel Bar]]></title><link><![CDATA[https://fushunharrislee.en.ec21.com/AISI_H13_DIN_1.2344_SKD61--11359578_11360647.html]]></link><description><![CDATA[is essential to cool the H13 slowly after forging, either in a furnace or in vermiculite.AISI H13 ANNEALING:Soak thoroughly at 840-860°C before furnace cooling at a maximum rate of 20°C per hour do]]></description><pubDate><![CDATA[20210331]]></pubDate></item>
<item>
<title><![CDATA[4340 Steel | 36CrNiMo4 | 1.6511 EN24 | 817M40 | SNCM439]]></title><link><![CDATA[https://otaisteel.en.ec21.com/4340_Steel_36CrNiMo4_1.6511_EN24--9723517_9833411.html]]></link><description><![CDATA[is essential to avoid the possibility of cracking.
Annealing of SNCM439 steel
The Slowly heated JIS SNCM439 to 830-860 ℃ and allow enough times, let the steel to be thoroughly heated, Then cool slo]]></description><pubDate><![CDATA[20160118]]></pubDate></item>