Search Advanced Search

Sell tzm rod, plate

  • Total 17 Related Items
  • Company Name :Luoyang Kekai Tungsten & Molybdenum Technology Co., Ltd.
  • Membership :Free member
  • Registrarion Date :2016. 04. 27
  • CountryRegion:China
  • Address:No.2205-2207, 11# Building, Yihaochengbang, Nanchang Road Luoyang Henan, China
  • Phone / Fax:0086-0379-65198702  /  0086-0379-65198121
  • Contact:Sandy Lee
Contact Now* Send an Inquiry to this supplier.
  • Share to :
  • Pinterest

Description

TZM alloy rod, molybdenum and zirconium-titanium alloy rods, titanium zirconium molybdenum alloy bar:

TZM alloy is a molybdenum-based alloys commonly used in a high-temperature alloys containing 0.50% titanium, 0.08% zirconium, the remaining 0.02% carbon molybdenum alloy.

TZM alloy rod advantages:
1) TZM alloy has good mechanical properties, in particular its mechanical properties are better than that of pure molybdenum at high temperatures. Table 2 (Ti0.5 / Zr0.1) TZM alloy mechanical properties, Table 3 TZM (Ti0.5-Zr0.08) the tensile strength and elongation at high temperatures.

2) TZM alloy (molybdenum zirconium-titanium alloy) also has good weldability, the material can be well H11 steel welding. Meanwhile TZM alloy is resistant to liquid metals such as Zn corrosion. It is cold-worked by conventional methods. In the case of cooling lubricants available cemented carbide or high speed steel cutting tools for machining.

TZM alloy (molybdenum zirconium-titanium alloy) and physical properties of pure molybdenum compared as follows:
Material   density /g•cm-3   Melting point /℃   Boiling point /℃
TZM alloy (Ti0.5/Zr0.1)   10.22   2617   4612
Mo   10.29   2610   5560

Mechanical Properties of TZM alloy (molybdenum zirconium-titanium alloy) (ri0.5 / Zr0.1) as follows:
Mechanical Properties  Elongation (%)  elasticity modulus GPa  Tensile strength Mpa   yield strength Mpa   fracture toughness MP•m1/2)
Value   <20   320   685   560-1150   5.8-29.6

TZM alloy (molybdenum zirconium-titanium alloy) high-temperature tensile strength and elongation:
Temperature   tensile strength(Mpa)   Elongation
RT    1140-1210  7.5-13.0
1000   700-720   5.2
1200   320-360   9.0
1300   190-210   11.5-13.5
1400   140-170   11-16

TZM alloy (molybdenum zirconium-titanium alloy) thermal performance and electrical properties:
Performance   coefficient of thermal expansion /K-1(20~100℃)   thermal conductivity W/m•K   Using maximum temperature in air ℃  ResistivityΩ•m
Value   5.3X10-6   126   400   (5.3~5.5)X10-8

Product Image

  • Sell tzm rod, plate

Browse: Manufacturer Directory Countries China India Korea Premium Suppliers Community Site Map

About EC21 Contact Us Terms & Conditions Report Item Online Trading Risks Product Listing Policy

中文 繁體 한국어 日本語 Español Русский Français Deutsch

Copyright (c)1997-2020 EC21 Inc. All Rights Reserved. EC21 in KoreanChinese

Business Registry Number: 120-86-03931

Inquiry Basket ()