Min. Order:
10000 Piece
Price:
US$ 0.5
Place of origin:
China
composition(%)
C:0.56-0.64, Mn:0.60-0.90, Si:1.60-2.00, Cr:≤0.35, P:≤0.03, S:≤0.03
C:0.56-0.64, Mn:0.40-0.70, Si:1.40-1.80,Cr:0.70-1.00 P:≤0.03, S:≤0.03
C:0.52-0.60, Mn:0.60-0.90, Si:1.50-2.00,Cr:≤0.35 P:≤0.03, S:≤0.03
C:0.35-0.42, Mn:0.50-0.80, Si:1.50-1.80, P:≤0.03, S:≤0.03
Hardness
For e clip: 44-48HRC
For skl clip: 42-47HRC
Fatigue life
for Dia.18 is 3 millions cycles with
[Related Keywords : SKL Rail CLip, SKL Tension Clip, SKL Rail Tension CLip, W Tension Clip]