Place of origin:
China
Supply Ability:
15000 permonth
Reduces silica film, Frorm CH4 from Sic
NITROGEN
1370℃
30
5
Form insulating Silicon Nitrides
PURE OXYGEN
1315℃
25
4
Faster oxidization than in air. Use LMA infusion glaze cotated starbar elements, or type TW, SE,SER or SEU
CO2
1500℃
25
4
No effect,may deposit Carbon
CO
1540℃
25
4
No effect
ARGON/HELIUM
1700℃
Maximum
Maximum
No detrimental effect
WATER DP 60°F
50°F
0 °F
-50 °F
1095
[Related Keywords : SiC, Heating Element, Heating Rod, Furnace]